Carte Re-based Diffusion Barrier on A Ni-based Superalloy Wang Yongming

Re-based Diffusion Barrier on A Ni-based Superalloy

Autor: Wang Yongming
Limbă: engleză
Legare: Carte broșată
Editura: Scholars' Press
Disponibilitate: În depozitul extern
Expediem în 5-8 zile
249.06 lei
The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat...

Informații despre carte

Limbă
engleză
Legare
Carte - Carte broșată
Publicat
2015
Pagini
204
EAN
9783639761023
ISBN
3639761022
Enbook ID
09198060
Editura
Greutate
304
Dimensiuni
152 x 229 x 12

Descriere completă

The gas turbine doubtlessly is one of the most important modern machines to convert energy from heat to power, and improving its efficiency is a ceaseless task. The most practical route to increase the efficiency is to increase the maximum operating temperature. Over the past several decades, the improvement of this temperature was constantly attained by the developments of thermal barrier coating and superalloys, but almost reached a limit because the microstructural deterioration of both the base superalloy and the coating system due to the interdiffusion between them can be dramatically aggravated by further increasing temperature. The novel diffusion barrier type bond coat, therefore, is a solution to this issue. This book introduces how to form a rhenium-based diffusion barrier on a nickel-based superalloy. The formation process and thermal stability of the diffusion barrier are discussed through analyzing its macro- and micro-structures by XRD, EBSD, EPMA, SEM, and TEM, etc. This work provides the fundamental knowledge about the novel coating system, and should be especially useful to researchers and students in high-temperature materials science and technology.

S-ar putea să te intereseze

143.47 lei
438.48 lei
1 100.75 lei

Aberdeen-Angus Herd Book, Volume 22

Aberdeen-Angus Cattle Society
218.63 lei
97.72 lei
70.72 lei
66.89 lei

Our Hadeland Ancestors - Volume 2

Hadeland Lag Of America
151.22 lei

Jo's Boys

Louisa May Alcott
90.17 lei

Little Women

Louisa Alcott
54.80 lei
18.43 lei

Passing the Torch

Derek Gallop
75.36 lei

Animal Farm

George Orwell
76.76 lei

The Christmas Pig

Joanne K. Rowling
103.47 lei
144.57 lei
79.28 lei
16.82 lei

Penthouse

Catherine Cooper
76.56 lei

Clienții care au cumpărat această carte au mai cumpărat și

I-Inthanethi

Owen Jones
27.50 lei
83.11 lei

Sweet Home T02

Youngchan Hwang
104.67 lei

Wer ist Der?

Heidemarie Kunze
42.41 lei

Leyendas

Gustavo Adolfo Bécquer
72.63 lei

Gül Yetistiren Adam

Rasim Özdenören
65.08 lei

Neue Theorie der Erde

Georg Christoph Silberschlag
105.99 lei
284.53 lei
60.85 lei
121.10 lei